What Is Heat Treatment in Steel? Annealing, Quenching, Tempering, and Carburizing Guide
What Is Heat Treatment in Steel? Annealing, Quenching, Tempering, and Carburizing Guide
Heat treatment in steel is a general term for controlled heating and cooling processes applied to steel materials to alter their mechanical properties—such as hardness, strength, toughness, wear resistance, and machinability. As explained in this Annealing, Quenching, Tempering, and Carburizing Guide, the correct heat treatment process can significantly increase the service life of a steel part, while an incorrect application can render it unusable.
At Uyar Çelik, with our half-century of experience in steel production, we offer our customers not only high-quality raw materials but also technical support in selecting and processing the right materials. In this guide, titled What Is Heat Treatment in Steel? Annealing, Quenching, Tempering, and Carburizing Guide, we detail the most commonly used heat treatment methods in the industry, their application parameters, and which treatment is suitable for which steel grade.
1. What is Heat Treatment and Why is it Necessary?
Heat treatment refers to thermal processes applied to steel to alter its internal structure (microstructure). Steel transforms into different crystal structures at different temperatures; these transformations are controlled to obtain the desired mechanical properties.
Basic Purposes of Heat Treatment
To increase hardness: For parts requiring wear resistance (gears, shafts, molds)
To increase strength: To provide higher load-carrying capacity
To improve toughness: To increase impact resistance by reducing brittleness
To facilitate machinability: To prepare for machining or cold forming
To relieve internal stresses: To reduce stresses that occur after welding, rolling, or forging
To homogenize the microstructure: To obtain consistent properties by smoothing the grain structure
Phase Transformations: Basic Concepts
| Phase | Formation Condition | Properties |
|---|---|---|
| Ferrite | Slow cooling | Soft, ductile, low hardness. The room-temperature structure of pure iron. |
| Pearlite | Slow cooling | A lamellar structure of ferrite and cementite. Offers medium hardness and strength. |
| Austenite | High temperature (>723°C) | Face-centered cubic structure. A paramagnetic phase capable of dissolving carbon. |
| Martensite | Rapid cooling (quenching) | Very hard and brittle. Forms by the sudden cooling of austenite. |
| Bainite | Moderate cooling rate | Properties between martensite and pearlite. Provides a good balance of hardness and toughness. |
| Cementite (Fe₃C) | Compound with carbon | Iron carbide. Very hard but brittle. |
2. Annealing
Annealing is the process of heating steel to a specific temperature, holding it at that temperature for a sufficient period, and then slowly cooling it (usually inside a furnace). The aim is to soften the steel, improve its machinability, and relieve internal stresses.
Types of Annealing
Full Annealing
Heated to 30–50°C above the upper critical temperature (Ac3) and slowly cooled in the furnace. The result is a fine-grained, homogeneous ferrite-pearlite structure. This process is particularly applied to correct the microstructure in castings and forgings.
Spheroidizing
In high-carbon steels (C > 0.6%), the hard and brittle cementite lamellae are spheroidized to improve machinability. The steel is held for an extended period just below or above the Ac1 temperature. Frequently applied to mold steels and spring steels.
Stress Relief Annealing
Performed to reduce internal stresses that occur after welding, machining, or cold forming. The steel is heated to 550–650°C, held at this temperature for 1–2 hours, and slowly cooled. There is no phase transformation; only stresses are relieved.
Homogenization Annealing (Diffusion Annealing)
This process is applied to eliminate chemical composition differences (segregation) that occur during casting. The steel is heated to high temperatures such as 1050–1200°C and held at this temperature for a long time. Then, normalization annealing is performed to refine the coarse grains.
Annealing Application Table
| Steel Grade | Temperature (°C) | Duration | Purpose |
|---|---|---|---|
| C45 (1.0503) | 800–850 | 1–2 hours | Machinability, stress relieving |
| 42CrMo4 (1.7225) | 820–860 | 1–2 hours | Softening, preparation for machining |
| 16MnCr5 (1.7131) | 830–860 | 1–2 hours | Preparation before carburizing |
| 100Cr6 (1.3505) | 780–810 | 2–4 hours | Spheroidizing annealing, machinability |
| S235/S355 | 550–650 | 1–2 hours | Post-weld stress relieving |
3. Normalization
Normalization is the process of heating steel to 30–50°C above its Ac3 temperature, holding it for a sufficient time, and then cooling it in still air. Unlike full annealing, cooling occurs in air, not in a furnace. The result is a finer-grained and slightly harder structure compared to annealing.
Purposes of Normalization:
To homogenize the irregular grain structure formed after rolling, forging, or casting.
To balance mechanical properties (strength + toughness).
To prepare for subsequent heat treatments (hardening, carburizing).
To be used as a final heat treatment in low and medium carbon steels.
Application: The normalization temperature for C45 steel is 840–870°C, and for 42CrMo4 it is 850–880°C. A holding time of approximately 1 hour is recommended for every 25 mm of part thickness.
4. Quenching / Hardening
Quenching is a fundamental method for achieving hardness in steel. The steel is heated to the austenitizing temperature (Ac3 + 30–50°C), held at this temperature, and then rapidly cooled (with water, oil, polymer, or air). Rapid cooling prevents the transformation of austenite into pearlite and allows the formation of a very hard martensite structure.
Cooling Media and Their Effects
| Medium | Cooling Rate | Hardness Effect | Application Area |
|---|---|---|---|
| Water | Very high | Maximum hardness | Carbon steels, low alloy steels |
| Oil | High | High hardness | Quenched and tempered steels (42CrMo4, C45) |
| Polymer | Adjustable | Controlled hardness | Precision parts, complex geometries |
| Air / Gas | Low | Medium hardness | High alloy steels, tool steels |
| Salt Bath | Medium | Uniform hardness | Small-section, alloyed parts |
Hardening Application Table
| Steel Grade | Austenitizing Temperature (°C) | Quenching Medium | Resulting Hardness |
|---|---|---|---|
| C45 | 820–860 | Water or oil | 55–58 HRC |
| 42CrMo4 | 830–860 | Oil | 54–58 HRC |
| 16MnCr5 | 830–860 | Oil | 60–62 HRC (surface) |
| 100Cr6 | 830–850 | Oil | 62–65 HRC |
| 1.2379 (D2) | 1000–1030 | Air or oil | 58–62 HRC |
| 1.2344 (H13) | 1000–1040 | Air or oil | 48–54 HRC |
5. Tempering
Tempering is a mandatory heat treatment applied immediately after quenching (hardening). The aim is to reduce the excessive brittleness of hardened steel and to establish an optimum balance between hardness and toughness.
Process: After quenching, the steel is reheated below the Ac1 temperature (between 150–650°C), held at this temperature for 1–2 hours, and cooled in air, oil, or water. As the tempering temperature increases, hardness decreases and toughness increases.
Tempering Temperature Ranges and Effects
| Temperature Range | Result | Typical Applications |
|---|---|---|
| 150–250°C | High hardness is retained, with a slight increase in toughness | Cutting tools, dies, bearings, measuring instruments |
| 250–400°C | Medium hardness, increased elasticity | Springs, pins, tools such as axes and knives |
| 400–650°C | Hardness decreases significantly, toughness reaches its maximum | Quenched and tempered steels (C45, 42CrMo4): shafts, gears, axles |
6. Improvement Process (Quenching + Tempering = Q&T)
Heat treatment is the combined application of quenching and tempering. The combination of hardening and high-temperature tempering (mostly 450–650°C) provides high strength, good toughness, and superior fatigue resistance.
Heat treatment takes its name from the “heat-treatable steels” specifically developed for this process. Medium-carbon, alloy steels such as C45, 42CrMo4, and 34CrNiMo6 belong to this group. Heat treatment is standard practice in shafts, axles, crankshafts, gearboxes, and machine parts requiring high strength.
Uyar Çelik’s range of high-quality steels such as C45, 42CrMo4, and 16MnCr5 have chemical compositions suitable for heat treatment. For a detailed comparison, please see our blog post “C45 vs 42CrMo4 vs 16MnCr5 Comparison”.
7. Cementation (Carburizing) — Surface Hardening
| Phase | Formation Condition | Properties |
|---|---|---|
| Ferrite | Slow cooling | Soft, ductile, low hardness. The room-temperature structure of pure iron. |
| Pearlite | Slow cooling | Lamellar structure of ferrite and cementite. Medium hardness and strength. |
| Austenite | High temperature (>723°C) | Face-centered cubic structure. A paramagnetic phase capable of dissolving carbon. |
| Martensite | Rapid cooling (quenching) | Very hard and brittle. Formed by the sudden cooling of austenite. |
| Bainite | Moderate cooling rate | Properties between martensite and pearlite. Good balance of hardness and toughness. |
| Cementite (Fe₃C) | Compound with carbon | Iron carbide. Very hard but brittle. |
Case-hardening steels
Case hardening is applied to low-carbon steels with a carbon content between 0.10% and 0.25%. Examples:
16MnCr5 (1.7131): The most common case hardening steel. Used in the production of gears, pins, and camshafts.
20MnCr5 (1.7147): Higher hardenability. Preferred in large-section gears.
18CrNiMo7-6 (1.6587): High performance. Used in aerospace and automotive transmission gears.
The surface hardness after case hardening is typically in the range of 58–63 HRC, while the core hardness remains around 30–40 HRC. The case hardening depth (CHD) is usually between 0.5–2.0 mm.
8. Other Surface Hardening Methods
8.1. Nitriding
Nitriding is a hardening process applied to the surface of steel by diffusion of nitrogen. Because it is applied at low temperatures such as 500–580°C, minimal deformation occurs in the part. Quenching is not required after nitriding; the surface hardens directly.
Surface hardness can reach 1000–1200 HV. Wear resistance, corrosion resistance, and fatigue strength are significantly increased. Steels containing aluminum, chromium, and molybdenum (such as 42CrMo4, 34CrAlNi7) are the most suitable grades for nitriding.
8.2. Induction Curing
Induction hardening is a process where the surface of a part is rapidly heated locally using an electromagnetic field, followed by quenching to harden it. Unlike carburization, it achieves hardness using only the existing carbon content without altering the chemical composition.
For induction hardening, the carbon content of the steel must be at least 0.35–0.50%. Medium carbon steels such as C45 and 42CrMo4 are ideal for this process. It is widely used in the automotive industry for hardening crankshafts, camshafts, gears, and shafts.
9. Which heat treatment is applied to which steel grade?
| Steel Grade | Steel Group | Recommended Heat Treatments |
|---|---|---|
| S235 / S355 | Structural | Normalizing, stress relieving annealing |
| C45 | Quenched & Tempered | Quenching & tempering, normalizing, induction hardening |
| 42CrMo4 | Quenched & Tempered | Quenching & tempering, nitriding, induction hardening |
| 16MnCr5 | Carburizing Steel | Carburizing + quenching, normalizing |
| 100Cr6 | Bearing Steel | Spheroidizing annealing, hardening + low tempering |
| 1.2379 (D2) | Cold Work Tool Steel | Hardening (air/oil) + multiple tempering |
| 1.2344 (H13) | Hot Work Tool Steel | Hardening + tempering (2–3 times), nitriding |
| 51CrV4 | Spring Steel | Quenching & tempering, stress relieving |
10. Common Mistakes and Precautions in Heat Treatment
Failure to Temper After Quenching
The most critical mistake. Quenched steel is extremely brittle and can crack suddenly during use. Tempering should be done as soon as possible after quenching (ideally within 1 hour).
Incorrect Temperature Selection
If the austenitizing temperature is too low, complete austenitization cannot be achieved, and hardness will be insufficient. If it is too high, grain coarsening occurs, and toughness decreases.
Insufficient Holding Time
It takes time to reach a homogeneous temperature to the center of the part. Insufficient holding time leaves untransformed areas in the center. As a general rule, a holding time of 1 hour should be applied for every 25 mm of wall thickness.
Incorrect Cooling Medium Selection
If carbon steel is quenched in oil, sufficient hardness may not be obtained. If alloy steel is quenched in water, excessive internal stress and cracking risk occur. Selecting a cooling medium appropriate to the steel grade is vital.
Oxidation and Decarburization
In heat treatment without a protective atmosphere, the steel surface oxidizes (scale forms) and loses carbon. This reduces surface hardness. Controlled atmosphere or vacuum ovens prevent this problem.
Frequently Asked Questions (FAQ)
Can heat treatment be applied to all types of steel?
No. For hardening, the steel must have a sufficient carbon content (usually min. 0.30–0.35%). Low-carbon structural steels (S235, S355) cannot be hardened; they can be subjected to normalization or stress-relieving annealing.
What is the difference between heat treatment and hardening?
Hardening (quenching) is a single-stage process aimed solely at achieving hardness. Heat treatment, on the other hand, is a combination of hardening and high-temperature tempering. Heat treatment provides both high strength and good toughness simultaneously.
What is the difference between cementation and nitriding?
In cementation, carbon is impregnated into the surface and then quenched with water (900–950°C). In nitriding, nitrogen is impregnated into the surface and quenching is not necessary (500–580°C). Since nitriding is done at a lower temperature, the risk of deformation is very low, but the hardening depth is shallower.
Which heat treatment should be applied to 42CrMo4 steel?
42CrMo4 is a heat-treatable steel. Standard application: austenitizing at 830–860°C → quenching in oil → tempering at 540–660°C. The result is a hardness of approximately 280–320 HB and high tensile strength (900–1100 MPa). Nitriding and induction hardening can also be applied.
Will the part change dimensions after heat treatment?
Yes. Dimensional changes are inevitable due to phase transformations and thermal expansion/contraction. Martensite formation causes approximately a 1% volume increase. Therefore, post-heat treatment planning, such as grinding or honing, should be done for precision parts.
Conclusion: What is Heat Treatment in Steel?
Heat treatment is a critical engineering process with the power to determine the performance of parts. Annealing for softening, normalization for homogenization, quenching for hardening, tempering for toughening, and carburizing for surface hardening—each addresses a different need.
The correct heat treatment application begins with the correct steel selection. At Uyar Çelik, with our half-century of experience, we produce heat-treatable steels, carburizing steels, and high-quality industrial steels in accordance with EN and ASTM standards. Our steel bars, produced in our modern facilities in Istanbul, Kocaeli, and Karabük, ensure consistent and reliable results for our customers in their heat treatment processes.

Let’s determine the right steel grade for your project together!
Uyar Çelik’s technical team will help you choose the most suitable steel grade for your heat treatment requirements. Contact us for technical consultation and a price quote on our range of heat-treatable steel bars.
Phone: